| Thermal Conductivity | 110-125W/mK |
|---|---|
| Porosity | 12-15% |
| Flexural Strength | 60 MPa |
| Coefficient Of Thermal Expansion | 5.2 X 10^-6 /K |
| Density | 1.85 G/cm3 |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 125 Mpa |
| Flexural Strength | 65 Mpa |
| Electric Resistance | 13~15 µΩ.m |
| Ash Content | 200/50 PPM |
| Bulk Density | 1.80 G/cm3 |
|---|---|
| Compressive Strength | 100 Mpa |
| Flexural Strength | 50 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 60 HSD |
| Bulk Density | 1.80 G/cm3 |
|---|---|
| Compressive Strength | 100 Mpa |
| Flexural Strength | 50 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 60 HSD |
| Flexural Strength | 50 MPa |
|---|---|
| Thermal Conductivity | 105 W/mK |
| Density | 1.81 G/cm3 |
| Purity | 99.95% |
| Thermal Expansion Coefficient | 5.4 X 10^-6 /K |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 105 Mpa |
| Flexural Strength | 55 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 65 HSD |
| Bulk Density | 1.80 G/cm3 |
|---|---|
| Compressive Strength | 100 Mpa |
| Flexural Strength | 50 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 60 HSD |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 105 Mpa |
| Flexural Strength | 55 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 65 HSD |
| Bulk Density | 1.80 G/cm3 |
|---|---|
| Compressive Strength | 100 Mpa |
| Flexural Strength | 50 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 60 HSD |
| Dimensional Stability | Excellent |
|---|---|
| Color | Dark Grey |
| Surface Finish | Smooth |
| Melting Point | 3650°C |
| Advantages | High Precision, Good Surface Finish, Long Tool Life |