| Thermal Conductivity | 110-125W/mK |
|---|---|
| Porosity | 12-15% |
| Flexural Strength | 60 MPa |
| Coefficient Of Thermal Expansion | 5.2 X 10^-6 /K |
| Density | 1.85 G/cm3 |
| Thermal Conductivity | 110-125W/mK |
|---|---|
| Porosity | 12-15% |
| Flexural Strength | 60 MPa |
| Coefficient Of Thermal Expansion | 5.2 X 10^-6 /K |
| Density | 1.85 G/cm3 |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 105 Mpa |
| Flexural Strength | 55 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 65 HSD |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 110 Mpa |
| Flexural Strength | 55 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 65 HSD |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 105 Mpa |
| Flexural Strength | 55 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 65 HSD |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 110 Mpa |
| Flexural Strength | 55 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 65 HSD |
| Melting Point | 3652°C |
|---|---|
| Purity | 99.9% |
| Shape | Powder |
| Material | Graphite |
| Hardness | 75 HS |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 110 Mpa |
| Flexural Strength | 55 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 65 HSD |
| Bulk Density | 1.72 G/cm3 |
|---|---|
| Compressive Strength | 85 Mpa |
| Flexural Strength | 42 Mpa |
| Electric Resistance | 13~14 µΩ.m |
| Shore Hardness | 60 HSD |
| Thermal Conductivity | 110-125W/mK |
|---|---|
| Porosity | 12-15% |
| Flexural Strength | 60 MPa |
| Coefficient Of Thermal Expansion | 5.2 X 10^-6 /K |
| Density | 1.85 G/cm3 |