| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 125 Mpa |
| Flexural Strength | 65 Mpa |
| Electric Resistance | 13~15 µΩ.m |
| Shore Hardness | 70 HSD |
| Particle Size | 6 Microns |
|---|---|
| Purity | 99.99% |
| Application Temperature | Up To 3000°C |
| Thermal Conductivity | 125 W/mK |
| Density | 1.85 G/cm3 |
| Particle Size | 6 Microns |
|---|---|
| Purity | 99.99% |
| Application Temperature | Up To 3000°C |
| Thermal Conductivity | 125 W/mK |
| Density | 1.85 G/cm3 |
| Bulk Density | 1.84 G/cm3 |
|---|---|
| Compressive Strength | 100 Mpa |
| Flexural Strength | 50 Mpa |
| Electric Resistance | 10~13 µΩ.m |
| Shore Hardness | 65 HSD |
| Bulk Density | 1.78 G/cm3 |
|---|---|
| Compressive Strength | 90 Mpa |
| Flexural Strength | 45 Mpa |
| Electric Resistance | 10~13 µΩ.m |
| Shore Hardness | 60 HSD |
| Bulk Density | 1.78 G/cm3 |
|---|---|
| Compressive Strength | 90 Mpa |
| Flexural Strength | 45 Mpa |
| Electric Resistance | 10~13 µΩ.m |
| Shore Hardness | 60 HSD |
| Bulk Density | 1.84 G/cm3 |
|---|---|
| Compressive Strength | 100 Mpa |
| Flexural Strength | 50 Mpa |
| Electric Resistance | 10~13 µΩ.m |
| Shore Hardness | 65 HSD |