| Bulk Density | 1.80 G/cm3 |
|---|---|
| Compressive Strength | 100 Mpa |
| Flexural Strength | 50 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 60 HSD |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 115 Mpa |
| Flexural Strength | 60 Mpa |
| Electric Resistance | 12~14 µΩ.m |
| Ash Content | 200/50 PPM |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 125 Mpa |
| Flexural Strength | 65 Mpa |
| Electric Resistance | 13~15 µΩ.m |
| Ash Content | 200/50 PPM |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 125 Mpa |
| Flexural Strength | 65 Mpa |
| Electric Resistance | 13~15 µΩ.m |
| Ash Content | 200/50 PPM |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 125 Mpa |
| Flexural Strength | 65 Mpa |
| Electric Resistance | 13~15 µΩ.m |
| Ash Content | 200/50 PPM |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 105 Mpa |
| Flexural Strength | 55 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 65 HSD |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 110 Mpa |
| Flexural Strength | 55 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 65 HSD |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 110 Mpa |
| Flexural Strength | 55 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 65 HSD |
| Bulk Density | 1.78 G/cm3 |
|---|---|
| Compressive Strength | 105 Mpa |
| Flexural Strength | 52 Mpa |
| Electric Resistance | 13~14 µΩ.m |
| Shore Hardness | 65 HSD |
| Bulk Density | 1.78 G/cm3 |
|---|---|
| Compressive Strength | 105 Mpa |
| Flexural Strength | 52 Mpa |
| Electric Resistance | 13~14 µΩ.m |
| Shore Hardness | 65 HSD |