| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 110 Mpa |
| Flexural Strength | 55 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 65 HSD |
| Bulk Density | 1.80 G/cm3 |
|---|---|
| Compressive Strength | 100 Mpa |
| Flexural Strength | 50 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 60 HSD |
| Flexural Strength | 50 MPa |
|---|---|
| Thermal Conductivity | 105 W/mK |
| Density | 1.81 G/cm3 |
| Purity | 99.95% |
| Thermal Expansion Coefficient | 5.4 X 10^-6 /K |
| Bulk Density | 1.80 G/cm3 |
|---|---|
| Compressive Strength | 95 Mpa |
| Flexural Strength | 48 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Shore Hardness | 60 HSD |
| Thermal Conductivity | 105-150 W/mK |
|---|---|
| Purity | 99% |
| Compressive Strength | 50-150 MPa |
| Density | 1.6-1.9 G/cm3 |
| Flexural Strength | 30-50 MPa |
| Thermal Conductivity | 105-150 W/mK |
|---|---|
| Purity | 99% |
| Compressive Strength | 50-150 MPa |
| Density | 1.6-1.9 G/cm3 |
| Flexural Strength | 30-50 MPa |
| Thermal Conductivity | 110-125W/mK |
|---|---|
| Porosity | 12-15% |
| Flexural Strength | 60 MPa |
| Coefficient Of Thermal Expansion | 5.2 X 10^-6 /K |
| Density | 1.85 G/cm3 |
| Thermal Conductivity | 110-125W/mK |
|---|---|
| Porosity | 12-15% |
| Flexural Strength | 60 MPa |
| Coefficient Of Thermal Expansion | 5.2 X 10^-6 /K |
| Density | 1.85 G/cm3 |
| Bulk Density | 1.85 G/cm3 |
|---|---|
| Compressive Strength | 115 Mpa |
| Flexural Strength | 60 Mpa |
| Electric Resistance | 13~14 µΩ.m |
| Shore Hardness | 70 HSD |
| Bulk Density | 1.80 G/cm3 |
|---|---|
| Compressive Strength | 100 Mpa |
| Flexural Strength | 50 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Ash Content | 500/50 PPM |