| Bulk Density | 1.78 G/cm3 |
|---|---|
| Compressive Strength | 90 Mpa |
| Flexural Strength | 45 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Ash Content | 500/50 PPM |
| Bulk Density | 1.76 G/cm3 |
|---|---|
| Compressive Strength | 85 Mpa |
| Flexural Strength | 45 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Ash Content | 500/50 PPM |
| Bulk Density | 1.76-1.80 G/cm3 |
|---|---|
| Compressive Strength | 85-95 Mpa |
| Flexural Strength | 45-50 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Ash Content | 50 PPM |
| Bulk Density | 1.76-1.80 G/cm3 |
|---|---|
| Compressive Strength | 85-95 Mpa |
| Flexural Strength | 45-50 Mpa |
| Electric Resistance | 11~13 µΩ.m |
| Ash Content | 50 PPM |